Filament Drying Calculator & Chart
Runs entirely in your browser — your numbers never leave your device.
Worked example
PETG at 60 °C for 5 hours in a 50 W dryer: 0.05 kW × 5 h = 0.25 kWh, about $0.05 at $0.18/kWh. Nylon is the long shift: 70–90 °C for 8–12 hours — start it the night before a big print, not the morning of.
How it works
Wet filament is the second most common cause of failed prints, and it disguises itself: popping and crackling at the nozzle, steam, stringing that no retraction setting fixes, rough or foamy surfaces, and layers that bond weakly and snap. If two or three of those show up together, dry the spool before changing any setting — the chart in this calculator follows the widely published dryer-maker figures for each material. Nylon is the extreme case: it absorbs moisture fastest and needs the longest, hottest dry, which is why nylon owners print straight from a dry box.
| Material | Drying temp | Time |
|---|---|---|
| PLA | ~45 °C | 4–6 h |
| PETG | 55–65 °C | 4–6 h |
| ABS / ASA | 60–80 °C | 4–6 h |
| TPU | 50–55 °C | 4–6 h |
| Nylon (PA) | 70–90 °C | 8–12 h |
Drying only resets the clock — storage decides how fast it runs out again. Keep spools sealed with desiccant between prints using the routine in our filament storage and drying guide, weigh suspect spools with the spool remaining estimator, and price what wet filament already cost you in the failed print cost calculator.
The formula: Recommended temperature and time come from the material lookup table above (published dryer-maker chart figures). Running cost = dryer watts ÷ 1,000 × hours × electricity rate.
Questions people ask
How do I know my filament is wet?
Listen at the nozzle: popping, hissing or tiny steam wisps are the classic signs, alongside new stringing, rough matte surfaces and weak layer bonding on a spool that printed fine before.
Can I dry filament in a food dehydrator or oven?
A dehydrator with accurate low temperatures works well. Ovens are risky — many cannot hold 45–60 °C accurately and can soften or fuse a spool. A purpose-built filament dryer is the safe default.
How long does a dried spool stay dry?
In open room air, PLA lasts weeks while nylon can pick up print-ruining moisture in a day or two. Sealed with desiccant, any material keeps for months.