Bed Adhesion: The Complete Fix List

The ranked list — work down it, not across it
Adhesion advice online reads like a raffle: glue! tape! hairspray! a new plate! Work through this list in order instead; each step is ranked by how often it turns out to be the real answer, and each is cheap or free until the last two.
- Wash the plate with dish soap and warm water. Skin oil is the number one cause, and alcohol wipes mostly smear it. This alone fixes the majority of 'suddenly nothing sticks' reports.
- Re-check the nozzle distance. A first layer that is not squished cannot grip. See the first layer guide for the ribbon test.
- Raise the bed temperature 5 °C. PLA grips best around 60 °C; PETG at 70–80 °C. A cold corner of a big bed can be the whole story on large parts.
- Slow the first layer and silence the fan. 20–25 mm/s, fan off for the first layers, first layer 5 °C hotter.
- Add a brim. 5–8 mm of sacrificial skirt multiplies the gripping area and is the specific cure for corners lifting.
- Kill the draft. A window, air-conditioning vent or opening door cools one side of the part; it shrinks, and the corner peels. Move the printer or shield it.
- Then, and only then, adhesives and surfaces — a glue-stick film, a fresh PEI sheet, or a purpose adhesion promoter.
Warping is adhesion losing an argument
Corners lifting mid-print is not the plate letting go for no reason — it is the part pulling itself off. Plastic shrinks as it cools; the top layers contract and curl the base upward with surprising force. Tall ABS and ASA parts are the extreme case (they genuinely need an enclosure), but big flat PLA parts warp too when a cold draft hits them. The counters are thermal: warmer bed, warmer room air around the print, a brim to hold the edges down, and rounded corners in the design where possible — sharp corners concentrate the pull.
Quotable fact: ABS shrinks roughly twice as much as PLA as it cools, which is why the same part that prints flat in PLA can curl dramatically in ABS on an open printer.
Know your surface
Smooth PEI grips PLA beautifully and can grip PETG too well — PETG has torn chunks out of smooth PEI and glass, which is why a glue-stick layer is used there as a release agent, not an adhesive. Textured PEI is the forgiving all-rounder most beginners should live on. Glass wants to be squeaky clean and hot. When a plate is genuinely worn — shiny patches, a visible ghost of every print — no cleaning revives it; plates are consumables and a fresh one is cheaper than a week of failed prints.
The small-print causes
A few adhesion mysteries have dull answers: the model is not actually touching the bed in the slicer (a 0.2 mm float ruins everything silently); the first-layer flow is under-extruding because of a partial clog (see the clog guide); or the filament is a PETG that wants a hotter bed than the PLA profile you sliced with. Check the profile matches the plastic — it is the 3D printing equivalent of 'is it plugged in', and it catches everyone once.
The two-print test that isolates the cause
When adhesion advice conflicts, run this experiment instead of arguing with the internet. Slice a simple 100 × 100 mm single-layer square — or use your printer's first-layer calibration file — and print it twice: once exactly as you have been, and once after a full dish-soap wash, a re-checked Z-offset and a 5 °C warmer bed, changing nothing else.
If the second print is perfect, your cause was in the trio you changed — and because they are the top three on the ranked list, that will be true most of the time. If it fails identically, your problem is mechanical or material: a bed with a genuine low spot, a mesh that is not being applied, or filament so wet it cannot grip. The test takes fifteen minutes and converts a fog of opinions into a fork with two branches. Every diagnosis in our guides follows this pattern — change the smallest set of things that can decide the question.
Adhesion by material: the plate pairings that work
Some combinations are simply marriages and some are feuds, and knowing the table saves plates. PLA on textured PEI is the beginner default for a reason — strong grip hot, releases as it cools. PETG on textured PEI is nearly as good; on smooth PEI or bare glass, use a glue-stick film as a parting layer or PETG may take the surface with it when it lets go — because eventually it lets go all at once.
ABS and ASA want a hot plate (95–110 °C) and still air more than any adhesive; on an open printer, a simple cardboard enclosure changes their behaviour more than any product. TPU grips almost everything too well — a glue film protects your plate from the part, not the reverse. Nylon is the diva: it barely respects PEI at all and traditionally wants a garolite (G10) surface or a purpose adhesive, printed straight from a dry box. If a material fights you at every step, check you are not asking a surface to do a job it was never paired for.
When to suspect the bed itself
Once in a while the plate is genuinely the problem, and it is worth knowing the evidence. Map the failure: if prints fail in the same region of the bed while succeeding elsewhere — the same corner releasing, the same patch refusing the first layer — suspect the surface or the bed's flatness rather than your technique. Run a large single-layer sheet and read it like a map: areas where lines separate sit low; areas where they scrape sit high. Automatic mesh levelling compensates for a lot, but it cannot compensate for a bed shaped like a crisp.
Plates also simply wear out. PEI coatings thin, textured surfaces polish smooth in the busy centre, and glass accumulates micro-scratches that change its grip. The honest lifespan of a hard-worked plate is measured in hundreds of prints, not thousands, and a fresh plate is one of the cheapest 'repairs' in the hobby. Before replacing, though, run the two-print test from this guide on a different area of the bed: if the fresh territory prints perfectly, rotate your printing to it while the new plate ships, and let the evidence — not frustration — make the purchase.
A note on first-layer squish vs elephant's foot
Chasing adhesion with ever more squish has a side effect worth knowing: the first layer spreads wider than the design, leaving a flared foot at the base of the part — elephant's foot. It matters on parts that must fit together precisely, and the cure is balance, not force: enough squish for a sealed, merged first layer, no more. Most slicers even carry an elephant-foot compensation setting that pulls the first layer's outline in by a tenth of a millimetre or two. If your parts grip beautifully but never quite fit, you have been over-squishing — back the offset up a hundredth at a time until the foot shrinks while the grip survives. Adhesion done properly is a window, not a maximum.
Common mistakes
- Reaching for glue before washing the plate.
- Printing PETG on smooth PEI with no release layer — it can take the surface with it.
- Blaming the plate when the slicer profile is for a different material.
- Using a raft on everything — it hides distance problems and wastes plastic; a brim is usually enough.
- Printing a huge flat part beside an open window in winter.
Printable quick-fix summary
- Wash plate: warm water + dish soap, dry, handle by edges.
- First layer: squished ribbon, 20–25 mm/s, fan off.
- Bed: PLA 60 °C · PETG 70–80 °C.
- Corners lifting → brim 5–8 mm + block drafts.
- PETG on smooth PEI/glass → glue stick as RELEASE layer.
Print this box (the page is print-styled for it) and keep it by the printer.
Opens the print dialog — choose “Save as PDF” and you get this guide as a clean BeginnerLayer PDF, masthead and all.
Questions people ask
Why did adhesion fail suddenly after weeks of success?
Almost always plate contamination building up, or a seasonal change — a colder room or a new draft. Wash the plate first; it is the answer far more often than any product.
Brim or raft — which should I use?
A brim for adhesion (it extends the part's own first layer). A raft only for very warped materials or uneven beds; it wastes plastic and leaves a rough bottom.
My print sticks too well and I can't remove it. Help?
Let the plate cool fully — PEI releases as it cools. Flex plates exist for this. A few minutes in the freezer releases stubborn PLA from glass.
Does bed temperature affect electricity cost much?
Barely — a heated bed draws tens of watts. The print cost calculator shows power is the smallest line in a print's true cost.