Shrinkage Compensation Calculator
Runs entirely in your browser — your numbers never leave your device.
Worked example
A 100 mm ABS calibration bar measures 99.4 mm in X and Y: 100 ÷ 99.4 × 100 = 100.60% scale on both axes — a 0.60% shrinkage, squarely inside the typical ABS range of about 0.4–0.8% in XY. Z barely moves (20 mm → 19.98 mm = 100.10%), which is normal: layers stack, they do not shrink the same way.
How it works
Plastic shrinks as it cools, and engineering plastics shrink most: a part designed at 100 mm can honestly print at 99.4 mm in ABS with nothing wrong with the printer. The fix is to print a plain test bar or cube at a known size, measure it cold with calipers, and enter the numbers here — per axis, because X and Y shrink with the material while Z is set by layer stacking and usually needs little or no correction. Enter the resulting scale percentages in your slicer's scale fields (OrcaSlicer/Bambu Studio and PrusaSlicer take per-axis scale on the object; Cura's scale tool does the same) or bake them into a material profile.
Two cautions keep this honest. First, the published material figures — ABS at roughly 0.4–0.8% in XY — are starting points, not constants: chamber temperature, brand and part geometry all move the real number, which is why the test print decides. Second, shrinkage compensation fixes overall size, not fit between two printed parts printed in different materials; for holes and mating parts, test the pair together. Size problems that change between prints are not shrinkage — check e-steps and belt tension first, and keep functional prints dry with the drying calculator.
The formula: Scale % (per axis) = target dimension ÷ measured dimension × 100. Shrinkage % = (target − measured) ÷ target × 100. Reference starting point: ABS shrinks roughly 0.4–0.8% in XY — verify with a test print.
Questions people ask
Why are X and Y different from Z?
XY dimensions are laid down as molten lines that contract as they cool. Z is built from stacked, already-cooling layers, so it shrinks far less — often near zero on a well-tuned machine.
Should I scale the model or use a slicer setting?
Either works — the maths is identical. A per-material slicer profile is cleaner if you print the same plastic often; scaling the model is fine for a one-off part.
Does PLA shrink too?
Much less than ABS — typically around 0.2–0.3% — which is why most PLA owners never notice it. It still matters on long, tight-tolerance parts.