Quick answer: Under-extrusion means less plastic is landing than the slicer asked for, leaving gaps, thin infill and weak walls. Diagnose by when it happens: only on fast sections = the hotend cannot melt fast enough; random with clicking = partial clog or slipping extruder; getting worse over a long print = heat creep. Start with the half-speed test — it splits the cause list in half for free.
Under-extrusion diagnosis infographic: gaps only at speed mean the hotend flow limit, random gaps with clicking mean a partial clog, worsening over time means heat creep, popping means wet filament — BeginnerLayer
When the gaps appear tells you where the starvation lives.

What under-extrusion looks like

The signs are consistent because the cause is simple: not enough molten plastic. Gaps between adjacent lines on top surfaces, sometimes with infill visible through pinholes. Walls that do not touch each other, so the part flexes and snaps cleanly along a layer when you bend it. Infill that looks like a fishing net instead of a solid lattice. A rough, pitted surface that feels starved rather than smooth. If instead the surface is bulging and ridged, you have the opposite problem — over-extrusion — and lowering flow is the right direction there. This page is about the starved print.

Under-extrusion has half a dozen common causes, and treating the wrong one wastes hours: raising flow to compensate for a partial clog works for two prints, then the clog finishes the job. So diagnose first. The single most useful clue is when the starvation appears.

When it happensMost likely causeFirst test
Only on fast sections — infill, long straight runsPrinting faster than the hotend can melt (volumetric flow limit)Reprint at half speed: gaps gone = flow limit
Random gaps, sometimes with extruder clickingPartial clog or extruder slippingExtrude 50 mm in mid-air: the strand should fall straight and even
Starts fine, gets worse over a long printHeat creep — filament softening too high in the hotendCheck the hotend cooling fan is at full speed
Popping, crackling, rough bubbly surfaceWet filament turning to steamDry the spool before changing anything else
Every print, every speed, by the same amountSettings: flow rate, filament diameter, or E-stepsCheck the slicer profile: 1.75 mm filament, flow at 100%
Began right after hotend work (Bowden machines)Gap between PTFE tube and nozzleRe-seat the tube hard against the nozzle

Quotable fact: Every hotend has a maximum melting rate measured in cubic millimetres per second — a standard hotend manages roughly 10–15 mm³/s, so wide lines at high speed can starve a print whose nozzle is perfectly clean.

Fix 1 — the speed test and the flow limit

Do this first because it costs nothing: reprint the same file at 50% speed. If the gaps vanish, your hotend simply cannot melt plastic as fast as the profile demands. The maths: flow = line width × layer height × speed. A 0.45 mm line at 0.2 mm layers moving 150 mm/s needs 13.5 mm³/s — near the ceiling of a standard hotend, and past it once the plastic is a high-temp or filled material. Cures, in order: raise nozzle temperature 5–10 °C (hotter plastic melts through faster), slow down the fast features (infill speed is the usual offender), or accept a thinner layer height on speed-critical prints. High-flow hotends exist precisely because this limit is real.

Fix 2 — the filament path, spool to gear

Walk the path the filament walks. Does the spool turn freely, or is a loop trapped under another loop, winching tighter as the print goes (this one gets worse and worse, then stops extrusion entirely)? Is the filament end's section in the extruder chewed into a notch with plastic dust around the gear — the gear has been slipping against resistance downstream, and grinding the filament is the symptom, not the disease. Is the extruder arm cracked? On many machines the plastic idler arm cracks underneath where you cannot see it, and the gear loses its grip pressure. Flex it and look. Our extruder clicking guide works this path in full — clicking and under-extrusion are usually the same fault announcing itself two ways.

Fix 3 — the nozzle: partial clog or worn bore

Extrude 50 mm of filament in mid-air at printing temperature. A healthy stream falls straight down at an even thickness. A stream that curls sideways the instant it leaves the nozzle, or comes out thin and sputtering, means a partial clog or a damaged orifice. Clear it with a cold pull — the full method is in our nozzle clog guide — and if the problem returns within a print or two on the same nozzle, replace it: brass nozzles are consumables, and abrasive filaments (glow-in-the-dark, wood-fill, carbon-fibre) can widen a 0.4 mm bore measurably in a single spool, after which no setting will make extrusion consistent again.

Fix 4 — heat creep, the slow starvation

Heat creep is the long-print killer: heat climbs the heat break, filament softens where it should still be rigid, swells, and drags — so extrusion gets worse the longer the print runs, classically 30–90 minutes in, and classically with PLA in a warm enclosure. The hotend cooling fan is the defence, and it must spin at full speed whenever the hotend is hot. A fan that starts lazily, ticks, or has a broken blade is a clog scheduled for next Tuesday. Also open the enclosure door for long PLA prints, and keep retraction distances sane — very long retractions drag melt into the cold zone where it freezes into a plug.

Fix 5 — only now, the settings

The volumetric budget, in plain numbers

It helps to see the ceiling as arithmetic. A standard 0.4 mm nozzle printing a 0.45 mm-wide line at 0.2 mm layer height lays down 0.09 mm² of cross-section; multiply by speed and you get demand: at 60 mm/s that is 5.4 mm³/s (comfortable), at 100 mm/s it is 9 mm³/s (near the standard hotend's practical ceiling), at 150 mm/s it is 13.5 mm³/s (past it — the infill gaps appear). Switch to a 0.28 mm 'draft' layer height and every one of those numbers grows by 40%: this is why the same printer that prints beautifully at 0.2 mm starves at 0.28 mm with unchanged speeds. High-flow hotends raise the ceiling to roughly 20–30 mm³/s, and larger nozzles raise demand faster than they raise supply — a 0.6 mm nozzle at speed is a flow-limit machine. When a print starves, do this maths for its fastest feature before touching any hardware.

Temperature buys flow, within limits: raising the nozzle 10 °C can add roughly 15–25% more melt capacity on common plastics, which is why 'hotter and slower' rescues draft-mode prints. Past the material's comfortable range, though, you are trading gaps for stringing, heat creep and degraded overhangs — the ceiling is real, and the honest options are speed, layer height, or a high-flow hotend.

Filament diameter: the quiet multiplier

One cause deserves a caliper before it earns a paragraph in most guides: the filament itself. Slicers assume the diameter you typed — almost always 1.75 mm — but real spools vary, and flow scales with the square of diameter. A spool measuring 1.70 mm delivers about 5.6% less plastic than the slicer expects; one at 1.68 mm is down 8% — squarely in visible-gap territory on top surfaces, on an otherwise perfect machine. Measure any suspect spool at several points along a metre (cheap filament can vary along its length, which prints as bands of alternating slight under- and over-extrusion), and if it sits consistently below 1.72 mm, either enter the measured diameter in the filament profile or retire the spool to non-critical prints. This is also why a printer can be 'calibrated' for one spool and starve on the next: nothing about the machine changed, but its raw material did.

With hardware cleared, check the numbers. Filament diameter in the slicer must say 1.75 mm if that is what is on the spool — a profile set to 2.85 mm silently scales every flow calculation down. Flow rate / extrusion multiplier belongs at 100% (0.95–1.0 in Bambu-style flow ratio) until you have a measured reason to move it. E-steps calibration is the last resort, and on modern machines with factory extruders it is rarely the answer: mark 100 mm of filament above the extruder, command 100 mm, and measure what actually fed. If it fed 100 mm, your settings were never the problem — go back to Fix 1–4. Use our filament calculators to sanity-check how much material a print should have used against what is left on the spool.

Common mistakes

Printable quick-fix summary

  • Half-speed test first: gaps gone = hotend flow limit, not a fault.
  • Mid-air test: 50 mm extruded straight and even = nozzle clear.
  • Check spool freedom, gear dust, cracked extruder arm.
  • Long-print starvation = heat creep: fan at full speed, door open for PLA.
  • Settings last: 1.75 mm diameter, flow 100%, then E-steps.

Print this box (the page is print-styled for it) and keep it by the printer.

Opens the print dialog — choose “Save as PDF” and you get this page as a clean BeginnerLayer PDF, masthead and all.

Questions people ask

What is the difference between under-extrusion and a clog?

A clog is one cause of under-extrusion — a restriction at the nozzle. Under-extrusion is the symptom (too little plastic) and can also come from speed beyond the hotend's melt rate, a slipping extruder, a tangled spool, heat creep or wrong settings.

Why does under-extrusion only happen on infill?

Infill prints fastest, so it is the first feature to exceed the hotend's volumetric flow limit. Walls, printed slower, stay under the limit and look fine. Raise temperature 5–10 °C or cap infill speed.

Can wet filament cause under-extrusion?

Yes — moisture flashes to steam in the nozzle, disrupting flow and leaving gaps, bubbles and a rough surface, often with popping sounds. Dry the spool (PETG 55–65 °C for 4–6 hours) before changing settings.

Should I just increase flow to 110%?

Only as a diagnostic: if 110% fixes it and hardware checks are clean, a small flow adjustment is legitimate. As a blind fix it over-extrudes everywhere else and hides a clog that will finish blocking mid-print.

Sources

Rate this guide & leave feedback

★ Reviews are moderated: comments appear publicly only after approval, so the page stays helpful and spam-free.